English

Free-Cutting Brass C85700

Versatile free-cutting brass offering excellent machinability and balanced properties for diverse industrial applications.

Material Introduction

Free-Cutting Brass C85700 is a high-performance leaded brass alloy specifically formulated for exceptional machinability in copper die casting applications. This versatile alloy combines excellent free-cutting characteristics with good mechanical properties and corrosion resistance, making it ideal for high-volume production of complex components requiring extensive machining operations. With its optimized lead content, C85700 produces small, fragmented chips during machining, which significantly reduces tool wear and increases production efficiency. The alloy exhibits good castability, along with smooth surface finish capabilities, making it suitable for a wide range of industrial applications. When processed through Neway's integrated tool and die making and precision post-machining services, it delivers reliable performance for architectural hardware, plumbing components, and industrial fittings.

Alternative Material Options

For applications requiring lead-free compliance while maintaining good machinability, Silicon Brass C87850 offers an excellent environmentally friendly alternative. When superior free-cutting performance is the primary requirement, Leaded Free-Cutting Brass C48500 provides the highest machinability rating. For general-purpose applications with good overall properties, Brass 360 serves as a reliable choice. In applications demanding higher strength and wear resistance, Aluminum Bronze C95400 delivers superior mechanical performance. For cost-sensitive projects that require reasonable machinability, Brass 380 offers a balanced solution. When considering non-copper alternatives, Zamak 5 zinc alloy offers good castability for small components.

International Equivalent / Comparable Grade

Country/Region

Equivalent / Comparable Grade

Specific Commercial Brands

Notes

USA (ASTM/UNS)

C85700 (Leaded Brass)

Mueller Brass C85700, PMX C85700, Concast C85700

Standard UNS designation for medium-leaded brass alloys.

Europe (EN)

CuZn39Pb0.5

KME CuZn39Pb0.5, Wieland CW510L, Luvata CuZn39Pb0.5

European brass grade with lower lead content but similar applications.

Japan (JIS)

C6782

JX Nippon C6782, Mitsubishi Shindoh C6782

Japanese brass standard with comparable machining characteristics.

Germany (DIN)

CuZn39Pb0.5

Diehl Metall CuZn39Pb0.5, Aurubis CuZn39Pb0.5

German specification matching European CW510L standards.

China (GB/T)

HPb63-0.1

Ningbo HPb63-0.1, Zhongse HPb63-0.1

Chinese brass grade with similar lead content and properties.

UK (BS)

CZ109 / CW510L

Luvata CZ109, Aalco CW510L

British standards aligned with European CW510L specifications.

Design Purpose

C85700 was specifically developed to bridge the gap between high-leaded free-cutting brasses and standard brass alloys, offering an optimal balance of machinability, mechanical properties, and cost-effectiveness. The alloy's composition was engineered to provide excellent chip formation during machining operations while maintaining sufficient strength and corrosion resistance for demanding applications. This design approach makes it particularly suitable for components that require both precise machining and reliable service performance. The alloy's versatility supports its use across multiple industries, from architectural hardware to industrial components, where efficient manufacturability and consistent quality are paramount. Its development focused on providing manufacturers with a reliable material solution that maximizes production efficiency while maintaining component integrity in metal casting applications.

Chemical Composition

Element

Copper (Cu)

Zinc (Zn)

Lead (Pb)

Iron (Fe)

Other Elements

Composition (%)

60.0-63.0

Balance

0.5-1.5

≤0.8

≤0.5 total

Physical Properties

Property

Density

Melting Range

Thermal Conductivity

Electrical Conductivity

Thermal Expansion

Value

8.4 g/cm³

900-930°C

105 W/m·K

24% IACS

20.8 μm/m·°C

Mechanical Properties

Property

Tensile Strength

Yield Strength (0.5%)

Elongation

Hardness

Machinability Rating

Value

380 MPa

170 MPa

22%

85 HB

90% (Very Good)

Key Material Characteristics

  • Excellent machinability with 90% rating compared to free-cutting brass standards

  • Good mechanical strength balanced with reasonable ductility

  • Superior chip formation during machining operations

  • Good corrosion resistance in various environments

  • Excellent castability with smooth surface finish capabilities

  • Maintains pressure tightness for fluid handling applications

  • Good wear resistance for moving components and fittings

  • Attractive golden appearance suitable for decorative applications

  • Cost-effective solution for high-volume production

  • Compatible with standard post-processing and finishing techniques

Manufacturability And Post Process

  • Copper Die Casting: Primary manufacturing process with excellent mold filling characteristics

  • Post Machining: Superior machinability enables high-speed drilling, tapping, and milling operations

  • CNC Machining: Ideal for complex geometries with tight tolerances (±0.025 mm)

  • Thread Cutting and Tapping: Produces clean, precise threads with extended tool life

  • Drilling and Boring: Excellent chip clearance enables efficient deep hole drilling

  • Tumbling: Effective for deburring and achieving uniform edge finishes

  • Sand Blasting: Creates consistent surface textures for aesthetic applications

Suitable Surface Treatment

  • Polishing and Buffing: Achieves high-luster finishes for decorative hardware

  • Clear Lacquering: Preserves natural brass appearance while preventing tarnishing

  • Electroplating: Compatible with nickel, chrome, and gold plating for enhanced durability

  • Powder Coating: Provides durable, colored finishes with proper surface preparation

  • Antique Patina: Chemical treatments create aged appearance for architectural applications

  • Passivation: Enhances corrosion resistance while maintaining metallic appearance

Common Industries and Applications

  • Architectural hardware, door handles, and decorative fittings

  • Plumbing fixtures and valve components

  • Industrial fittings and machinery components

  • Electrical connectors and electronic hardware

  • Marine hardware and coastal architectural elements

  • Consumer product components and hardware

  • Lock mechanisms and security hardware

When to Choose This Material

  • High-volume machining applications: Excellent machinability reduces production time and costs

  • Complex threaded components: Superior chip formation enables clean, precise threading

  • Architectural and decorative hardware: Attractive appearance with good machining characteristics

  • Cost-effective production: Balanced performance at competitive material costs

  • Plumbing and industrial fittings: Good corrosion resistance and pressure tightness

  • Components requiring extensive post-machining: Extended tool life reduces manufacturing costs

  • General-purpose brass applications: Versatile performance across multiple industries

Explore Related Blogs

Copyright © 2026 Diecast Precision Works Ltd.All Rights Reserved.