CuZn10

Ductile low-zinc brass offering excellent corrosion resistance, smooth surfaces, and reliable performance for precision cast components.

Material Introduction

CuZn10 is a low-zinc brass alloy engineered for precision copper die casting and machining applications where excellent ductility, corrosion resistance, and surface quality are required. With approximately 10% zinc and a high copper balance, CuZn10 exhibits superior formability and stable mechanical behavior compared with higher-zinc brasses. Its clean microstructure supports smooth casting surfaces and predictable machining, making it well suited for fittings, valve components, decorative hardware, electrical connectors, and thin-wall mechanical parts. When combined with Neway’s controlled melting practice and optimized tool and die making, CuZn10 delivers reliable dimensional accuracy and consistent cosmetic quality across medium-to-high production volumes.

Alternative Material Options

If higher strength and wear resistance are needed, CuZn37 or CuZn40 provide increased hardness at the expense of ductility. For improved machinability in threaded parts, Leaded Free-Cutting Brass C48500 is often selected. Where corrosion resistance in potable water or low-lead compliance is critical, Silicon Brass C87850 offers a suitable alternative. For bearing or sliding applications, Leaded Bronze C83600 provides superior lubricity, while higher-strength service may justify Aluminum Bronze C95400.

International Equivalent / Comparable Grade

Country/Region

Equivalent / Comparable Grade

Specific Commercial Brands

Notes

Europe (EN)

CuZn10 (CW501L)

Wieland CW501L, Aurubis CW501L

Standard low-zinc brass with high ductility.

USA (ASTM)

C22000

Olin C220, Mueller C220

Commercial bronze; closest functional equivalent.

China (GB/T)

H90

Chalco H90, Nanshan H90

Common low-zinc brass for fittings and hardware.

Japan (JIS)

C2200

UACJ C2200, Mitsubishi C2200

Equivalent composition used in precision components.

UK (BS)

CZ101

Avon CZ101

Traditional designation aligned with CuZn10 chemistry.

Design Purpose

CuZn10 was designed to prioritize ductility, corrosion resistance, and surface finish rather than maximum strength. Its low zinc content minimizes stress-corrosion susceptibility and provides stable performance in water, mild chemicals, and atmospheric exposure. Designers choose CuZn10 for thin-section castings, intricate fittings, and visible components where uniform appearance, reliable sealing, and ease of secondary forming are essential. The alloy supports light mechanical loading while maintaining excellent aesthetic quality, making it a strong choice for architectural, plumbing, electrical, and consumer hardware.

Chemical Composition

Element

Copper (Cu)

Zinc (Zn)

Lead (Pb)

Iron (Fe)

Other

Composition (%)

~89–91

~9–11

≤0.05

≤0.05

Trace

Physical Properties

Property

Density

Melting Range

Thermal Conductivity

Electrical Conductivity

Thermal Expansion

Value

~8.8 g/cm³

~930–970 °C

~120–140 W/m·K

~28–30% IACS

~19–21 µm/m·°C

Mechanical Properties

Property

Tensile Strength

Yield Strength

Elongation

Hardness

Value

~250–320 MPa

~90–120 MPa

~25–35%

~70–90 HB

Key Material Characteristics

  • Excellent ductility and formability for thin-wall castings.

  • High corrosion resistance in water and atmospheric environments.

  • Smooth as-cast surface suitable for decorative finishing.

  • Low susceptibility to stress-corrosion cracking.

  • Good electrical and thermal conductivity.

  • Stable machining behavior with clean surface finish.

  • Good soldering and brazing compatibility.

  • Balanced cost for copper-rich precision components.

Manufacturability And Post Process

  • Copper die casting: CuZn10 fills dies smoothly due to its copper-rich composition, supporting thin sections and fine details in precision copper die casting.

  • Gravity and sand casting: Suitable for larger or lower-volume components where uniform solidification and surface quality are required.

  • CNC machining: Performs well on CNC machining centers, enabling tight tolerances on sealing faces, threads, and mating features.

  • Drilling and threading: Clean chip formation allows accurate threads and smooth bore finishes.

  • Deburring and finishing: Tumbling or light brushing removes minor burrs and prepares surfaces for coating or assembly.

  • Inspection: Dimensional checks and surface inspection are applied to ensure cosmetic and functional consistency using Neway’s inspection equipment.

Suitable Surface Treatment

  • Polishing: Achieves bright, decorative finishes for visible components.

  • Clear lacquer or protective coating: Prevents oxidation and color change.

  • Nickel or chrome plating: Enhances wear resistance and appearance.

  • Powder coating: Provides durable color finishes for consumer and architectural hardware.

  • Bead blasting: Produces uniform matte texture prior to coating.

  • Laser marking: Enables permanent identification without affecting corrosion performance.

Common Industries and Applications

  • Plumbing fittings and valve components.

  • Electrical connectors and terminals.

  • Architectural and decorative hardware.

  • Light-duty mechanical fittings and couplings.

  • Consumer hardware requiring clean surface finish.

When to Choose This Material

  • When high ductility and corrosion resistance are required.

  • When thin-wall casting and smooth surfaces are design priorities.

  • When electrical or thermal conductivity is beneficial.

  • When decorative appearance matters alongside functional reliability.

  • When low-lead or cleaner brass chemistry is preferred.