中文

Za 8

ZA-8 is a zinc-aluminum alloy offering high strength, excellent wear resistance, and tight dimensional control for industrial die-cast applications.

Introduction to ZA-8

ZA-8 (Zinc Aluminum Alloy 8%) is a hypoeutectic zinc-based casting alloy with approximately 8.4% aluminum content, specifically engineered for high-strength and high-precision die-cast components. It provides superior hardness, excellent dimensional stability, and improved wear resistance compared to traditional Zamak alloys.

As part of the zinc-aluminum die casting alloy group, ZA-8 is suitable for gravity and pressure die casting and can also be machined, plated, and easily polished. At Neway Die Casting, ZA-8 is utilized in components where tight tolerances, mechanical strength, and bearing properties are critical.

ZA-8 Chemical Composition

Element

Weight %

Function

Zinc (Zn)

Balance

Base metal

Aluminum (Al)

8.0–8.8

Strengthens alloy, improves wear resistance

Copper (Cu)

0.8–1.3

Increases hardness and bearing characteristics

Magnesium (Mg)

0.015–0.03

Enhances strength, reduces oxidation

Iron (Fe)

≤ 0.075

Impurity control

Tin (Sn), Nickel (Ni), Lead (Pb), Cadmium (Cd)

≤ 0.003 each

Impurities minimized per ASTM B86 standards

Physical Properties of ZA-8 Alloy

Property

Value & Unit

Density

6.3 g/cm³

Melting Range

381–390 °C

Thermal Conductivity

109 W/m·K

Electrical Conductivity

~27 % IACS

Coefficient of Thermal Expansion

~25 µm/m·°C

Specific Heat Capacity

~400 J/kg·K

High density and thermal conductivity make ZA-8 ideal for parts exposed to thermal cycling and dynamic loads.

Mechanical Properties (As-Cast & Aged)

Property

Typical Value & Unit

Ultimate Tensile Strength

350 MPa

Yield Strength

280 MPa

Elongation

1–3 %

Brinell Hardness

100 HB

Impact Strength (Notched Izod)

~3.5 J

Modulus of Elasticity

~96 GPa

These values exceed those of Zamak 3 and Zamak 5, making ZA-8 suitable for structural and load-bearing components.

Castability of ZA-8

ZA-8 is unique among zinc alloys in that it is suitable for both pressure die casting and gravity casting. It has:

  • Excellent dimensional control (linear shrinkage <0.006 mm/mm)

  • High casting fluidity, allowing for thin walls and complex geometries

  • Low hot tearing tendency

  • Improved wear resistance compared to Zamak series

At Neway’s zinc casting facility, ZA-8 is cast using thermal-balanced dies and monitored fill speeds to achieve tight dimensional tolerances without distortion.

Common Applications

ZA-8 is widely used in applications requiring strength, surface finish, and machinability:

  • Automotive: Transmission and drivetrain brackets, timing covers

  • Consumer electronics: Connector housings, lens mounts

  • Office equipment: Bearings, bushings, levers

  • Functional prototyping for zinc structural parts

  • Furniture and mechanical assemblies with sliding motion and wear zones

Machining Challenges and Solutions

While ZA-8 is more machinable than aluminum alloys, its high aluminum content makes it harder than Zamak, leading to increased tool wear:

  • Use of carbide or TiCN-coated tools is recommended

  • Proper lubrication prevents chip welding and edge buildup

  • Clamping and vibration control is essential for precision features

Neway integrates CNC post-machining and quality control (CMM + visual inspection) to ensure surface finishes of Ra 1.6 µm and dimensional tolerances of ±0.03 mm.

Surface Treatment Compatibility

ZA-8 offers superior surface finish post-casting and is compatible with multiple secondary finishes:

Its surface structure supports high adhesion strength for coatings and plating, allowing long-term durability even in humid environments.

FAQs

  1. How does ZA-8 differ from Zamak 3 in mechanical strength?

  2. Can ZA-8 be used for gravity casting processes?

  3. What is the maximum wall thickness suitable for ZA-8 pressure die casting?

  4. Is ZA-8 recommended for parts requiring long-term dimensional stability?

  5. Does ZA-8 require post-aging to reach optimal mechanical properties?

探索相关博客